Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of RADIFLAM S RV300 HFL 5138 OR - PA6-GF30 - RadiciGroup High Performance Polymers

Material Data Center offers the following functions for RADIFLAM S RV300 HFL 5138 OR:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Radiflam S datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
PA6 flame retardant injection moulding grade, halogen and red phosphorus free. 30% glass fibre reinforced. Orange colour (comparable to RAL 2003) stable at high temperature.

Suitable for parts requiring fire retardancy along with high stiffness and good mechanical resistance. Good electrical insulating properties. Laser markable grade. Rated V-0 according to UL-94.
Processing/Physical Characteristics건조/응축단위시험규격
ISO 데이터
성형 수축률, 평행 0.2 / * % ISO 294-4, 2577
성형 수축률, 수직 0.6 / * % ISO 294-4, 2577
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 11200 / - MPa ISO 527
파단시 강도 115 / - MPa ISO 527
파단시 신율 2 / - % ISO 527
챠피 충격 강도 , +23°C 40 / - kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 7 / - kJ/m² ISO 179/1eA
열적 특성건조/응축단위시험규격
ISO 데이터
녹는점, 10°C/min 220 / * °C ISO 11357-1/-3
두께 H인 제품의 난연성 V-0 / * class IEC 60695-11-10
테스트 두께 0.8 / * mm -
전기적 특성건조/응축단위시험규격
ISO 데이터
부피 저항 1E13 / 1E11 Ohm*m IEC 62631-3-1
표면 저항 * / 1E10 Ohm IEC 62631-3-2
CTI 600 / - - IEC 60112
기타 특성건조/응축단위시험규격
물에서의 흡수성 4.4 / * % ISO 62와 유사
조건에서의 흡습성 1.2 / * % ISO 62와 유사
밀도 1460 / - kg/m³ ISO 1183
특징
생산 공정
사출 성형
인도 유형
과립
부가물
이형제
특별 특성
난연성, Halogen-free, Phosphorus-free, 열안정성
특성
Laser Markable
지역별 검색
기타 정보
사E성
The material is delivered in moisture-proof packaging ready for processing. Maximum recommended water content for best processing is 0.10%. Typical conditions with a desiccant drier: temperature 80 ° C, dew point -20 ° C or below, time 2-4 h or more. Avoid excessive shear rates and high thermal stresses for better processing. Special care must be taken to avoid moisture absorption and contamination with other polymers when adding regrind material. Colour variation and mechanical properties reduction may occur and should always be carefully monitored.

Injection Molding Processing Parameters
Melt Temperature Mold Temperature Injection Speed
250 - 280°C 80 - 100°C medium-high
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com